PETROL STEEL CO., LTD. supplies Inconel 625 seamless pipe, UNS N06625, made to ASTM B444 and ASME SB444. The pipe is cold-drawn, annealed, or solution annealed and pickled, in outside diameters from 1/2 in to 6-5/8 in (12.7 to 168 mm), with walls to standard schedules or by agreement. Alloy 625 is a nickel-chromium-molybdenum-niobium alloy, and it is the material engineers move to when 316L has pitted, duplex has cracked, and 825 has run out of margin. We work with EPC contractors, engineering consultants, and plant procurement teams, and our quotations follow the way those teams actually buy: the grade is stated, the certificates are agreed, and the inspection hold points are written down before production starts. Typical uses are chemical injection and instrument and process lines in offshore, sour gas, and chemical plants, where a small pipe carries a large consequence. The heat number on the pipe matches the certificate, and we state it in the quotation instead of leaving it to be assumed. If your datasheet calls for “Alloy 625,” “N06625,” “NCF 625,” or “2.4856,” this page sets out what B444 requires, what we add on top of it, and what we need from you to quote.
| Item | Specification |
|---|---|
| Standard | ASTM B444 / ASME SB444, general requirements, ASTM B829 |
| Grade | UNS N06625 (Inconel 625, Alloy 625, W.Nr. 2.4856, NCF 625), Grade 1 or Grade 2 |
| Process | Seamless, cold-drawn, annealed (Grade 1) or solution annealed (Grade 2), pickled |
| Size | OD 1/2–6-5/8 in (12.7–168 mm), NPS 1/4–6, as listed in B444 Appendix X1; other sizes on enquiry |
| Wall thickness | SCH 10S, 40S, 80S, 160, XXS, or special wall by agreement |
| Length | Single random 5–7 m, double random 10–14 m, or cut to length |
| Ends | Plain end, square cut, or beveled for welding |
| Certificates | EN 10204 3.1 as standard, 3.2 with a third-party witness |
| Inspection | Hydrotest or eddy-current test on every piece, PMI; UT, grain size, ASTM G28 and G48 on request |
What ASTM B444 Covers, and a Common Mix-Up
B444 covers cold-worked seamless pipe and tube in three alloys: UNS N06625, N06852, and N06219. General requirements for tolerances, sampling, and test procedures are in ASTM B829. The 2023 revision also deleted the dimensions and permissible variations section from B444 itself, so a datasheet that quotes tolerances “per B444” is working from an older edition. Ordering follows clause 4.1: alloy or UNS number, ASTM designation, condition, finish, dimensions, length, quantity, test type, certification, and any supplementary requirement. Three supplementary requirements, S1 to S3, apply only when the buyer asks for them, and they are covered below. Small-diameter converter sizes, meaning tubes up to 1-1/4 in OD with a wall of 3% of OD or less, are listed in Annex A1 and ordered by OD and wall, not by pipe schedule. One mix-up appears in inquiries more than any other. Some buyers cite B423 for Alloy 625 pipe. B423 is the specification for Alloy 825 (N08825), which we cover on our Incoloy 825 seamless pipe to ASTM B423 page, while Alloy 625 pipe is made to B444. If the wrong standard is put on a purchase order, the mill certificate will not match the line item, which is a poor thing to discover at a client audit. Welded Alloy 625 pipe falls under B705 and fittings under B366, so keep seamless pipe, welded pipe, and fittings on separate lines of the material take-off.
Grade 1 or Grade 2: The Decision That Drives the Order
B444 splits N06625 into two grades, and the buyer has to choose one. Grade 1 is annealed at a minimum of 1600°F (871°C) and is normally used up to 1100°F (593°C). Grade 2 is solution annealed at a minimum of 2000°F (1093°C), with an optional stabilization anneal at a minimum of 1800°F (982°C) to improve resistance to sensitization; it is normally used above 1100°F where creep and rupture strength matter. Table 1 allows Grade 2 to be solution annealed with or without that second anneal, so state on the order whether you want the stabilization step. Grade 1 is the stronger of the two at room temperature, which surprises people who assume the hotter heat treatment means higher strength. If a purchase order names neither grade, B444 says Grade 1 is supplied, so a line that runs hot must say Grade 2 in writing. The hydrotest allowable fiber stress follows the grade as well: 30,000 psi (207 MPa) for Grade 1 and 25,000 psi (172 MPa) for Grade 2. When a datasheet gives us a design temperature, we compare it with the grade before quoting, and we raise the question if the two do not agree.
| UNS N06625 | Heat treatment | Normal service | Tensile, min | Yield 0.2%, min | Elong., min. |
|---|---|---|---|---|---|
| Grade 1 | Annealed, 1600°F (871°C) min | Up to 1100 °F (593 °C) | 120 ksi (827 MPa) | 60 ksi (414 MPa) | 30% |
| port, | port, | Above 1100°F, creep and rupture | 100 ksi (690 MPa) | 40 ksi (276 MPa) | 30% |
Minimum support: the values apply to tubing in straight lengths. Tensile properties do not apply below 1/8 in (3.2 mm) OD or 0.015 in (0.38 mm) wall. Hot-forming quality is furnished only to chemistry and surface inspection; no mechanical properties are required.
Chemistry and Corrosion Performance of UNS N06625
The B444 chemistry explains the alloy’s reputation. Nickel is at least 58.0%, and chromium is 20.0% to 23.0%. Molybdenum at 8.0 to 10.0% and niobium plus tantalum at 3.15 to 4.15% strengthen the matrix, giving the alloy strength without precipitation hardening and increasing resistance to pitting and crevice attack. Carbon is held to 0.10% maximum and iron to 5.0% maximum. In service, this has four practical consequences. Pitting and crevice corrosion in warm seawater and chloride brines is far better controlled than in 316L or 825. Chloride stress corrosion cracking is rarely the limiting factor at temperatures where austenitic stainless steel fails. Resistance to many acids and to mixed H₂S and CO₂ environments is high, which is why 625 is used in sour gas service within the limits of NACE MR0175 / ISO 15156; we confirm the condition and hardness against your datasheet instead of assuming compliance. The alloy also maintains its strength at temperatures where 825 starts to lose margin. Grade matters here as well: the chemistry is identical, but the heat treatment changes strength and creep behavior. Typical density is 8.44 g/cm³, and the typical melting range is 1290–1350°C. We report the actual heat analysis on every certificate, not only the limits.
| Element | Limit, % | Element | Limit, % |
|---|---|---|---|
| Nickel | 58.0 min | Niobium + tantalum | 3.15–4.15 |
| Chromium | 20.0–23.0 | Iron | 5.0 max |
| Molybdenum | 8.0–10.0 | Carbon | 0.10 max |
| Cobalt (if determined) | 1.0 max | Manganese | 0.50 max |
| Silicon | 0.50 max | Aluminum | 0.40 max |
| Titanium | 0.40 max | Phosphorus | 0.015 max |
| Sulfur | 0.015 max |
Where Inconel 625 Seamless Pipe Is Specified
Alloy 625 pipe is usually specified where a failure is expensive to reach, expensive to repair, or both. Offshore and subsea work uses it for chemical injection, instruments, and seawater lines on platforms and FPSOs. Upstream gas uses it for sour gathering lines, wellheads, and manifold piping. Chemical and petrochemical plants specify it for heat exchangers, reactor lines, and acid service; power and environmental projects for flue gas desulfurization and scrubber piping; and desalination and geothermal plants for hot brines. Demand follows the project calendar: gas processing in the Middle East; offshore developments off Brazil, West Africa, and the North Sea; Gulf Coast chemical retrofits; and new capacity across Southeast and Central Asia. A significant share of 625 piping is small-bore, such as instrumentation, injection, and sampling lines, which suits cold-drawn seamless pipe well. Retrofit and replacement work matters as much as new build: corroded 316L and carbon steel lines in older plants are often replaced with 625 during shutdowns, when the schedule leaves little room for a second round of certificate questions. For EPC contractors, the commercial questions repeat from project to project: will the certificate package pass the client audit, can the material be inspected before shipment, and will the price hold long enough to award the order? We build every quotation around those three points.
Quality Control and Inspection
B444 sets a baseline. It requires one chemical analysis and one tension test per lot and a hydrostatic or nondestructive electric test on every piece, at the manufacturer’s option unless the purchase order names one. The hydrotest applies from 1/8 in OD upward with a wall of 0.015 in or more and may be taken to one and a half times the allowable fiber stress by agreement. Anything beyond that must be written into the order, and the standard’s three supplementary requirements are the ones we recommend for critical service. S1 sets average grain size at ASTM 5.0 or finer, determined on each heat treatment lot under ASTM E112. S2 is the ASTM G28 Method. An intergranular corrosion test, with a maximum rate of 0.003 ipm (0.914 mm/yr). S3 is the ASTM G48 Method C pitting and crevice test at 75°C for 72 hours, with no visible pitting deeper than 0.001 in (0.025 mm) at 20× and a weight loss below 1.0 g/m². None of them apply unless the order says so. In addition to the standard, every pipe is traced to its heat number, mill test certificates follow EN 10204 3.1 (3.2 with a third-party witness), and positive material identification confirms the alloy before packing, because nickel alloys are easy to confuse on a rack. UT, or eddy-current testing, is available on request, and we welcome SGS, BV, TÜV, or your inspector at the mill, with hold points agreed upon before production, not afterward.
Inconel 625 vs. Incoloy 825 vs. 316L, and Welding the System
Most inquiries carry one cost question: is 625 really necessary? The table sets the three common choices side by side. As a rule, choose 316L when the medium is mild and chlorides are low, Alloy 825 when acids or hot chlorides would crack or pit 316L, and Alloy 625 when seawater, crevice conditions, temperature, or strength exceed what 825 can handle. Price per kilogram is rarely the only consideration, because one failed 316L line in seawater service costs more in lost production than the premium for the right alloy. Welding is straightforward if the shop is disciplined. Use matching filler such as ERNiCrMo-3, keep heat input low, and maintain clean interpass conditions. Field failures are rarely metallurgical; they come from carbon steel contamination, grinding dust, and chain slings. Use dedicated stainless or nickel-alloy tools, store pipe on timber or stainless racks, and pickle after welding where the specification calls for it. Pipe is rarely ordered alone, and the fitting side of the same alloy is on our Inconel 625 butt weld fittings to ASTM B366 WPNCMC page, so pipe and fittings can be specified against the same alloy and certificate requirements.
| Property | 316L | Alloy 825 | Alloy 625 |
|---|---|---|---|
| Seamless pipe standard | ASTM A312 | ASTM B423 | ASTM B444 |
| Nickel content | About 10–14% | 38–46% | 58% min |
| Molybdenum content | About 2–3% | 2.5–3.5% | 8.0–10.0% |
| Pitting and crevice resistance | Moderate | Good | Excellent |
| Chloride stress corrosion cracking | Low resistance | High resistance | Very high resistance |
| Strength at elevated temperature | Limited | Moderate | High |
| Relative material cost | Lowest | Medium | Highest |
Packing, Delivery, and How to Request a Quotation
Pipes are packed in plywood cases or bundled with end caps and non-metallic spacers, marked with the standard, grade, heat number, and size as your order requires, and shipped FOB or CIF to your port. Nickel alloy pricing follows the LME nickel price, so our quotations carry a validity period; tell us your award date, and we will price to it. Send OD, WT, grade & quantity, and state whether you need Grade 1 or Grade 2, which of S1 to S3 apply, the certificate type, any third-party inspection requirement, the destination port, and your project specification. We will return a clear offer covering price, lead time, MOQ, documentation, and inspection plan. Lead time depends on size and stock and is confirmed in the quotation, and so is the MOQ. We keep the datasheet response, the certificate package, and the inspection plan in one reply so your team can forward it straight to the client. If the datasheet is still open on grade or standard, send it as it is, and we will go through it with you before the quotation, not after.
INCONEL is a registered trademark of Special Metals Corporation. Alloy names are used on this page only to identify the material grade. PETROL STEEL CO., LTD. is an independent supplier.
C. FAQ (Top 8)
Q1. Is Inconel 625 seamless pipe made to ASTM B423 or ASTM B444?
ASTM B444. ASTM B444 and ASME SB444 cover UNS N06625 seamless pipe. B423 is the specification for Alloy 825 (UNS N08825) pipe and tube. If your inquiry cites B423 for Alloy 625, send us the datasheet, and we will confirm the correct standard before quoting.
Q2. What is the difference between Grade 1 and Grade 2 Inconel 625 pipe?
Grade 1 is annealed and normally used up to 1100 °F (593 °C), with minimums of 120 ksi tensile and 60 ksi yield. Grade 2 is solution annealed and normally used above 1100°F where creep and rupture strength matter, with minimums of 100 ksi tensile and 40 ksi yield. If the order names neither grade, B444 says Grade 1 is supplied.
Q3. Is Inconel 625 suitable for sour gas (H₂S) service?
Yes, Alloy 625 is widely used in sour gas gathering and wellhead piping. Compliance with NACE MR0175 / ISO 15156 depends on the material condition, hardness, and service limits, so we will confirm it against your datasheet before quoting.
Q4. Should I choose Inconel 625 or Incoloy 825 pipe?
Choose 825 for acids and moderate chloride service where cost matters. Choose 625 for seawater, severe pitting and crevice conditions, higher temperatures, or higher strength. Alloy 625 costs considerably more, so we compare both against your datasheet before recommending one.
Q5. What sizes of Inconel 625 seamless pipe can you supply?
B444 Appendix X1 lists cold-drawn pipe from 1/2 in to 6-5/8 in (12.7 to 168 mm) OD, all schedules. Larger sizes or heavier walls depend on mill capability, and welded pipe to ASTM B705 may be the alternative. Send OD and WT, and we will confirm the route.
Q6. What certificates and tests do you provide?
EN 10204 3.1 mill certificates as standard, and 3.2 when a third party witnesses the tests. B444 requires one chemical analysis and one tension test per lot and a hydrostatic or nondestructive electric test on every piece. Grain size (S1), ASTM G28 intergranular corrosion (S2), and ASTM G48 pitting (S3) tests apply only when written into the order. PMI is done before packing, and SGS, BV, or TÜV inspection can be arranged.
Q7. How do I weld Inconel 625 pipe?
Use a matching filler such as ERNiCrMo-3, with low heat input and clean interpass conditions. Avoid contamination from carbon steel and grinding dust, and pickle after welding where specified.
Q8. What do you need to quote, and how is nickel price volatility handled?
Send OD, wall thickness, grade (1 or 2), quantity, destination port, and project specification. Prices follow LME nickel, so our offers carry a validity period set to your award date.